Why Thermoforming Film Tears or Thins at the Corners

Oct 13, 2026

Leave a message

Film-side causes

Film formulation may not suit the draw. Nylon (PA) contributes toughness and puncture resistance, while metallocene PE can improve toughness in the PE layers. In our supply experience, differences in formulation and layer ratio can explain why films with the same structure name behave differently. A lower price alone does not identify the cause of tearing.

Thickness may need adjusting. A film that works for a shallow pocket may leave weak corners in a deeper pack. We compare the starting thickness with the application and any previous successful film. Our thickness guide gives experience-based ranges for initial sample selection.

Not enough toughness for the journey. When packs survive forming but break in transport, look at the nylon content and total thickness against the product weight and the distribution route.

Machine-side checks

Ask the machine operator or equipment supplier to check the following alongside the film. These checks help separate a film issue from a change in forming conditions:

Heating temperature and time: check for uneven heating or settings outside the recommended range for the film.

Forming vacuum or pressure: insufficient or unstable forming force affects how the film fills the corners.

Mould condition: damaged edges, sharp corners or residue can tear the film locally.

Recent changes: new settings, a new mould or maintenance work since the last good run.

Quick reference

 

 

Symptom

Check on the film

Machine or handling check

Tears during forming

Film formulation and layer ratio compared with the last satisfactory run

Heating temperature and time; mould edges

Thin or weak corners

Starting thickness against pocket depth

Heating evenness; forming vacuum or pressure

Breaks in transport

Nylon content and total thickness

Pack design, fill and handling

 

A practical way to find the cause

Compare the failing run with the last satisfactory one, noting any changes to the film, product or machine settings. If the film changed, share the old and new specifications with the supplier. If the machine settings changed, ask the operator or equipment supplier to review them. Test one change at a time and compare the finished packs.

 

Thermoformed pack with a torn corner

Selecting samples to investigate the problem

Send us the product, approximate pocket depth, current film structure and thickness if known, and photos showing where and when the pack fails. A machine model or a previous film specification is useful if available. We can suggest sample options based on these details. Test them on your line and share the forming, sealing and handling results so we can review the film choice with you.